Prepreg 1080 vs Prepreg 2116: Key Differences in PCB Design

Introduction

Choosing the right materials is crucial in PCB design, especially when it comes to laminates. In this article, we’ll explore Prepreg 1080 vs Prepreg 2116, guiding you through their differences in structure, application, and performance to help you make an informed decision for your next PCB project.

What is a Prepreg?

Prepreg, short for “pre-impregnated,” is a dielectric material used extensively in multilayer PCB fabrication. It consists of woven glass fibers combined with a resin binder, typically epoxy, and is positioned between two cores or between a core and a copper foil. Once pressed and heated during lamination, the prepreg cures and bonds the layers, ensuring structural integrity and electrical insulation.

Prepreg serves both mechanical and electrical functions in PCB fabrication. Mechanically, it holds the PCB layers together. Electrically, it insulates them, preventing signal interference and short circuits.

Certain prepregs also allow for selective conductivity. When plated through holes are drilled, conductive paths form where needed, while the surrounding areas maintain insulation. This controlled conductivity is essential for reliable multilayer interconnections.

Prepreg-PCB
Prepreg-PCB

How Prepregs Are Manufactured

Prepregs are manufactured using two main processes: the solvent dip process and the hot melt process. Each method is selected based on the type of prepreg being produced and the material requirements.

The solvent dip process is typically used for fabric-based prepregs. In this method, the resin is first dissolved in a solvent. The reinforcing fabric is then passed through the resin solution, allowing it to absorb the resin uniformly. After dipping, the material is dried in an oven to remove the solvent, leaving behind resin-coated fibers that are partially cured.

The hot melt process, on the other hand, is more versatile. It is used for both unidirectional and fabric prepregs. This method involves a two-step procedure. A thin layer of resin is created through heating. This layer is then mixed with the reinforcement material in the prepreg machine. By applying heat and pressure, the resin thoroughly soaks into the fibers. The result is a controlled, partially cured prepreg material ready for PCB lamination.

Prepreg Manufacturing
Prepreg Manufacturing

Prepreg 1080 vs Prepreg 2116 Differences

You can see both Prepreg 1080 vs Prepreg 2116 in  PCB manufacturing. But they perform and behave differently. You need to know how they differ before you choose one. Each affects how your PCB will work and last.

Thickness and Resin Content

Prepreg 1080 is thinner than Prepreg 2116. It measures around 60 to 70 microns. Prepreg 2116 is thicker—about 90 to 110 microns. Prepreg 1080 also has more resin, around 60% by weight. Prepreg 2116 has about 50%. This changes how they bond and insulate. Thicker prepregs support stronger builds, but may hold less resin.

Storage Conditions and Shelf Life

Storage time matters. Prepreg 1080 lasts longer on the shelf. It holds up better at room temperature, around 23°C. Prepreg 2116 has a shorter life span. If you’re not using the material quickly, 1080 is a safer pick. Just make sure to keep both in a dry, cool place.

Testing Method

To measure resin content, a burnout test works for both but will have different result. You heat the sample, burn off the fiber, and weigh what’s left. The weight change shows the resin amount. Remember that different brands also result to different Df/Dk so perform a burnout test if possible. This helps you compare actual content between Prepreg 1080 vs Prepreg 2116, which affects bonding and flow.

Temperature and Handling Recommendations

Keep both below 23°C and away from moisture. Use gloves. Don’t fold or crease the sheets. The 1080 prepreg, with its looser weave, is easier to work with. The 2116’s tighter weave makes it stronger but less flexible. Handle accordingly.

Cost

Prepreg 2116 costs more than Prepreg 1080. Its added thickness and lower resin load make it more expensive. If your design doesn’t demand thick dielectric spacing, 1080 can help you save money. Use 2116 only if your stack-up needs more height or support.

Prepreg 1080 vs Prepreg 2116
Prepreg 1080 vs Prepreg 2116

Advantages of Prepregs in PCB Manufacturing

Improved Process Control

One of the standout benefits of using prepregs is how they help create a cleaner and more controlled processing environment. Since the resin is already infused into the reinforcement fabric, you can skip the manual resin application altogether. This means you can place the layers precisely without worrying about resin overflow or inconsistencies, which not only boosts efficiency but also cuts down on cleanup time.

Reduced Curing Time

Prepregs require only a single heat curing cycle. Once the cycle is finished up, the parts are all set for post-processing or assembly. This cuts down on the long wait times that come with full wet lay-up cure schedules, which can drag on for as long as 48 hours

Improves Uniformity and Consistency

Prepregs offer great consistency and uniformity thanks to their reliable fiber and resin content. Once you peel off the backing films and stack the plies, the layup process becomes pretty straightforward. Plus, curing and vacuum bagging are easier than resin infusion, which leads to more predictable outcomes.

Improved Mechanical Properties

The right balance of fiber to resin in prepregs really boosts mechanical strength. This careful mix makes it possible to create composite structures that are stiffer, more durable, and lighter—qualities that are essential for high-performance applications.

Co-Curing Capability

Prepregs make it possible to cure multiple layers or components at the same time, a process known as secondary or co-curing. This technique leads to stronger interlaminar bonds and enhances the overall structural integrity of the materials.

Prepregs in PCB Manufacturing
Prepregs in PCB Manufacturing

Issues You May Face on Using Prepregs

Higher Material and Processing Costs

Prepregs are generally more expensive than combining dry fabric with liquid resin systems. This cost difference is due to their precise manufacturing process, which involves controlled resin content, uniform impregnation, and cleanroom environments. Additionally, curing prepregs typically requires specialized equipment such as autoclaves or programmable convection ovens, further increasing production costs.

Limited Shelf Life

Prepregs have a finite shelf life, typically around six months under room temperature conditions. Exposure to elevated temperatures can accelerate resin advancement, degrading performance. To maintain usability, prepregs are often stored in refrigerated or frozen environments to delay curing and preserve material quality. While some variations exist in shelf life depending on the formulation, cold storage is standard practice in ensuring prepreg integrity over time.

Heat Cure Requirements

Prepregs require a controlled heat cure process for proper resin polymerization. Manufacturers must maintain a consistent temperature, often around 270°F (132°C), for a sustained period—typically at least four hours. This thermal requirement makes autoclaves or high-performance ovens essential for achieving optimal mechanical properties and bonding. The reliance on heat cure systems can limit prepreg use in settings without such equipment.

Prepregs Issues
Prepregs Issues

Choosing Prepreg for PCB Design

When selecting prepreg during PCB design, fabric weight and resin content matter a lot. Lightweight fiberglass with higher resin creates smooth, resin-rich surfaces. It helps with filler distribution and finer copper etched patterns. Heavier fabrics cost less and offer better dimensional stability. They also allow thicker boards at a lower cost. Heavy fabrics like 7628 prepreg can affect smoothness and drilling. It can cause small drills to break or defect.

When it comes to prepreg types like 106, 1080, 2116, 2313, and 7628, you’ll find that they differ in thickness and resin content depending on the supplier. You’ll also find standard, medium, and high resin versions. Prepregs are chosen depending on PCB thickness, stack-up, dielectric constant, dimensional stability, and budget. Thicker prepregs usually cost more. Like copper clad laminates, prepregs come in high Tg and halogen-free options, though not all thicknesses are available.

Prepreg for PCB Design
Prepreg for PCB Design

Other Types of Prepregs

Thermoplastic and thermoset are two other main types of prepregs.

Thermoplastic prepregs are made from fiberglass that’s soaked in thermoplastic resins such as PPS, PP, PEEK, PE, and PET. You can find these prepregs in various forms, including woven, stitched, or unidirectional. Unlike thermoset prepregs, thermoplastic prepregs remain stable at room temperature but generally have a shorter shelf life.

Thermoset prepregs are more common in composite manufacturing, with epoxy being the primary resin. Other thermoset resins include phenolic and BMI. Initially, the resin is liquid when it impregnates the fiber reinforcement. Excess resin is removed, and the epoxy partially cures to a tacky solid state known as the “B-stage.” At this stage, the resin is semi-solid but not fully hardened. When heated further, the resin liquefies again before fully curing and becoming cross-linked. This final cure provides the strong, rigid bond essential for high-performance prepregs.

PCB Layout
PCB Layout

FAQs

  • What Material Is PCB 1080?

PCB 1080 is a type of E-glass fabric prepreg used in multilayer PCB manufacturing. It consists of woven glass fiber impregnated with partially cured resin, which allows the material to bond and insulate layers during lamination. The 1080 fabric provides mechanical strength and helps define the board’s thickness and electrical properties like impedance. This prepreg is essential for ensuring the structural integrity and performance of multilayer PCBs.

  • What Is the Standard Thickness of Prepreg?

The standard thickness of prepreg used in printed circuit boards (PCBs) typically ranges from 0.002 to 0.024 inches (0.05 to 0.6 mm). Common thicknesses include 0.002″, 0.004″, 0.006″, 0.008″, 0.010″, and 0.012″. For high layer count PCBs, even thinner prepregs are available, sometimes as thin as 0.0005″ (0.0127 mm), to accommodate complex designs.

  • Why Is Prepreg Used In PCB?

Prepreg plays a crucial role in PCB manufacturing, acting as the insulation material that holds the layers together in a PCB stack-up. It connects cores to other cores or layers while providing essential electrical insulation to avoid short circuits. This fiberglass fabric, soaked in resin, not only secures the multiple layers tightly but also maintains the board’s structural integrity. During the manufacturing process, prepreg is applied and fused under heat and pressure, resulting in a solid, cohesive board. Additionally, it shields the resin and fiberglass from moisture and environmental harm, boosting the board’s durability and overall performance.

Conclusion

This PCBMay article compared Prepreg 1080 vs Prepreg 2116, highlighting their differences in thickness, resin content, storage, handling, and cost. It explained how these factors affect PCB performance and manufacturing. The discussion also covered prepreg advantages, limitations, and guidance on choosing the right material for specific PCB design needs.

If you’re looking for multilayer PCBs made with premium Prepreg 1080 vs Prepreg 2116, PCBMay is your trusted partner. Contact PCBMay today for expert manufacturing, top-quality materials, and customized solutions that meet your exact specifications. Let PCBMay bring your PCB designs to real PCB boards with unmatched precision and reliability.

Scroll to Top

Get a Quick Quote!

x
Upload File

Get a Quick Quote!

x
Upload File